An elastomeric bearing pad is the flexible element placed between a bridge superstructure and its substructure. It carries vertical load, absorbs rotation and permits horizontal movement, while damping the vibration that traffic sends into the deck. For most highway, pedestrian and rail structures the material decision comes down to two families of rubber: natural rubber (NR) and chloroprene rubber (CR), widely known as neoprene. Both are elastic, both are robust, and both can be produced as plain pads or as laminated bearings with bonded steel reinforcement. They are not, however, interchangeable in every application. Temperature, ozone exposure, expected service life and the surrounding environment all push the selection one way or the other. This guide compares NR and CR on the points that actually decide a project, and sets out a repeatable way to choose between them.
Getting the material right matters more than many designers expect, because the bearing is one of the few components that cannot easily be replaced once the bridge is in service. A pad that hardens prematurely, cracks at the edges or relaxes under sustained load will change how the whole structure behaves. Selecting the correct elastomer at the drawing stage is therefore a structural decision, not a purchasing formality.
An elastomeric bearing pad is a shaped block of vulcanised rubber that works in compression, shear and rotation. In its simplest form it is a plain pad with no reinforcement, used where loads are moderate and rotations are small. Where higher loads or larger rotations are expected, the rubber is laminated with thin steel plates bonded between layers of elastomer. The steel prevents the rubber from bulging sideways under load, raising the vertical stiffness while keeping the pad flexible in shear.
Because the pad deforms rather than resists, it accommodates thermal expansion of the deck, concrete creep and shrinkage, and the small rotations caused by live load without transferring damaging forces into the abutment or pier. That behaviour is why the elastomer grade — not just the pad dimensions — is treated as a design variable rather than a commodity detail.
The geometry of the pad and the properties of the rubber always work together. Two pads of identical size but different compounds can behave very differently under the same load, which is why specifications treat material, hardness and geometry as a single package.
Natural rubber is produced from latex and is prized for its outstanding elasticity, high tensile strength and excellent fatigue resistance. It recovers quickly after repeated deformation, which suits structures that experience many load cycles. Its weakness is environmental: unprotected NR is attacked by ozone and by oils and solvents, and it hardens progressively at low temperature.
Chloroprene rubber is a synthetic polymer whose molecular structure includes chlorine. That single difference gives CR markedly better resistance to ozone, weathering, heat ageing and hydrocarbons. CR also performs better than NR in cold conditions and resists flame far more effectively. The trade-off is cost and a slightly lower resilience at very low strain.
In practice, the choice is rarely about strength. It is about the environment the bearing will live in for decades and about how much of the service life must be delivered without intervention. A bridge in a sheltered inland valley and a bridge on an exposed coastal viaduct may carry identical loads yet deserve different elastomers.
It also helps to separate two questions that are often merged. The first is whether the elastomer can carry the load; both NR and CR can. The second is whether it will still behave predictably after years of weather, ozone and temperature cycling. That second question is where the two materials genuinely diverge.
The table below summarises the differences that matter most during selection. Values are general engineering guidance and should always be confirmed against the governing project specification.
| Property | Natural rubber (NR) | Chloroprene rubber (CR / neoprene) |
|---|---|---|
| Base polymer | Natural latex | Synthetic polychloroprene |
| Elasticity and recovery | Excellent | Very good |
| Fatigue resistance | Excellent | Very good |
| Ozone and weathering resistance | Moderate without protection | Excellent |
| Low-temperature flexibility | Limited, stiffens in cold | Better cold performance |
| Heat ageing | Moderate | Good |
| Oil, fuel and solvent resistance | Poor | Good |
| Flame resistance | Poor | Good |
| Typical climate fit | Mild, stable climates | Cold, coastal or polluted sites |
Read the table as a set of tendencies rather than a scorecard. A well-compounded NR pad can serve for decades in a benign climate, while CR earns its premium where ozone, salt air or temperature swing would shorten an NR pad's life. When a project sits between the two, the decision usually turns on how conservative the owner wants to be about maintenance access.
Hardness deserves a separate note. Both NR and CR are supplied across a range of hardness values, and hardness can be tuned independently of the base polymer. A harder CR compound and a softer NR compound are both possible, so "NR versus CR" and "soft versus hard" are two different decisions that must be made together.
Temperature sets the practical envelope for any elastomer. As rubber cools it stiffens, and below a certain point it can become glass-like and lose the flexibility the bearing depends on. NR loses flexibility earlier than CR, which makes it a weaker candidate for structures in severe winter conditions or where the bearing is exposed to wind chill on an elevated deck.
At the warm end of the scale the concern reverses. Heat accelerates ageing, and NR ages faster than CR when sustained elevated temperatures are combined with oxygen and ozone. A dark, sun-exposed bearing on a southern-facing deck therefore behaves quite differently from a sheltered one, even at the same ambient temperature.
Humidity and airborne pollution add a third variable. Coastal sites carry chloride-laden air, and industrial corridors can carry ozone and hydrocarbons. In both cases CR's chemistry gives it a clear advantage over unprotected natural rubber.
Altitude, shading and the colour of adjacent surfaces can also shift the effective temperature a bearing experiences. A pad in permanent shade may age more slowly than one a few metres away in full sun, which is one reason blanket rules of thumb should be checked against the actual exposure of each support.
Short-span pedestrian bridges in temperate regions frequently use plain or lightly laminated NR pads, where the pads are lightly stressed and the climate is kind. Highway bridges in cold climates, structures near the coast, and decks exposed to de-icing salts or industrial pollution are more often specified with CR or an NR grade protected against ozone.
Where rotations and loads are large, the same material logic is applied inside a laminated or pot bearing rather than a plain pad, because the reinforcement changes how the elastomer is loaded and restrained. For a wider view of the bearing families available for different structural situations, see the full bridge bearing range.
Two practical rules help narrow the field early. First, match the material to the climate the bearing will actually experience, not the climate at the design office. Second, decide whether the structure can tolerate an intervention during its design life; if it cannot, the more weather-resistant elastomer is usually the safer choice.
A third rule is to think about the whole set of supports rather than one. It is often simpler for maintenance if a bridge uses one elastomer family throughout, even if a single sheltered support could have used the cheaper option. Consistency on site has real value over a long service life.
Material selection is only defensible when it is tied to a recognised specification. In North America, ASTM D4014 sets out the requirements for plain and steel-laminated elastomeric bearings used in bridges, covering the elastomer grades and the physical properties they must meet. Its public summary can be reviewed at ASTM D4014.
In Europe and in many markets that follow European practice, BS EN 1337-3 covers elastomeric structural bearings and defines material and performance requirements that designers can reference directly for both NR and CR compounds. The published scope is described at BS EN 1337-3.
Whichever specification governs a project, the elastomer grade, hardness and any protective treatment should be stated on the drawing and verified against the delivered bearings. Writing the requirement down is what turns a good material decision into a reliable structure, and it gives everyone on site a single, unambiguous reference to work from.
Yes. Neoprene is the trade name most engineers use for chloroprene rubber (CR). When a drawing specifies neoprene bearing pads, it is calling for a polychloroprene elastomer of the kind described above.
They can, and sometimes are, when different locations have different exposure. A sheltered interior support and an exposed coastal abutment can reasonably carry different elastomers, provided each is specified correctly and clearly marked on the drawings.
Steel laminations restrict the lateral bulge of the rubber, which increases vertical stiffness without removing the flexibility needed to accommodate rotation and shear. That combination is what allows a relatively thin bearing to carry a heavy load.
No. Hardness is one of several properties that must be balanced with elasticity, relaxation and fatigue behaviour. A stiffer compound that resists rotation too strongly can transfer unwanted forces into the structure.
By matching the specified grade to a recognised standard, and by keeping the material requirement on the approved drawing so that it can be checked against the bearings supplied.
Generally no. Once a bearing has been loaded and unloaded, its properties and internal condition cannot be assumed to be unchanged, and it is normally replaced rather than reinstalled.
Selecting between NR and CR is a decision that benefits from a second opinion grounded in real structures. Share the span, the design loads, the rotation, the climate and the governing specification, and the material choice, hardness and bearing type can be narrowed quickly and defensibly.
Discuss Your Elastomeric Bearing Pad Requirements

Water-Filled Rubber Dam: 5 Field Failures That Show Up Before the Dam Bag Bursts
Bridge Bearing Pad Design for Bridge Construction: Load Transfer, Movement and Reliable Service
Bridge Bearing Pad Inspection and Maintenance: A Field Guide for Safer Bridge Construction
Bridge Bearing Pad Inspection: Movement, Damage and Maintenance Records